TerlouwRoofing · Utrecht, home

Roofs in Utrecht.

275 m² of roof in six neighborhoods. For each job: what was wrong, what we did and how long it took.

  1. bitumen loose at the edge1upstand only 6 cm high2damp patch in bedroom3
    upstand 15 cm above the tiles1EPDM 1.14 mm, fully bonded2tiles on adjustable pedestals3
    BeforeAfter
    1. bitumen loose at the edge
    2. upstand only 6 cm high
    3. damp patch in bedroom

    Lombok

    Flat roof under a roof terrace replaced

    Area
    28 m²
    Duration
    2 days
    Material
    EPDM

    Before

    The old bitumen under the tiles had come loose at the seams. When it rained, a wet patch showed up in the bedroom below.

    After

    Tiles off, new EPDM in one piece, upstands raised 15 cm and the tiles put back on pedestals.

    New build-up, top to bottom

    • Concrete tiles 60 × 60 × 4 cm on adjustable pedestals
    • Rubber protection mat 6 mm
    • EPDM 1.14 mm, fully bonded, upstand 15 cm above the tiles
    • Existing 100 mm insulation with vapor barrier
    • Plywood 18 mm on 71 × 196 mm joists
  2. lead flashing cracked1stain above the closet2
    lead code 20, dressed per tile1new joint to dormer roof2
    BeforeAfter
    1. lead flashing cracked
    2. stain above the closet

    Wittevrouwen

    Leak at a dormer repaired

    Area
    6 m²
    Duration
    1 day
    Material
    Lead and bitumen

    Before

    Water ran in along the side wall of the dormer. The stain was a meter away, above the closet.

    After

    Replaced the lead flashing on the side and redid the joint with the dormer's flat roof.

    New build-up, top to bottom

    • Code 20 lead (2 mm), worked in tile by tile along the side wall
    • Lead apron under the window frame, over the tiles
    • Dormer roof: two layers of SBS bitumen up to the roof trim
    • Ceramic tiles on 22 × 32 mm battens
  3. no insulation1condensation on the ceiling2
    120roof edge raised 12 cm1PIR 120 mm · Rd 5.4522 layers of SBS bitumen3
    BeforeAfter
    1. no insulation
    2. condensation on the ceiling

    Leidsche Rijn

    Flat roof of a business unit insulated

    Area
    120 m²
    Duration
    5 days
    Material
    PIR and bitumen

    Before

    Uninsulated roof with gravel. Condensation on the inside in winter and a high heating bill.

    After

    Gravel off, 120 mm PIR insulation, two layers of bitumen and the gravel put back around the rooftop units.

    New build-up, top to bottom

    • Gravel 16/32, 50 mm layer
    • SBS bitumen cap sheet 4 mm, base sheet 3 mm
    • PIR 120 mm, Rd 5.45
    • Vapor barrier with aluminum layer
    • Roof edge raised 12 cm, new roof trim
  4. six tiles gone1water in the attic2
    new concrete tiles1ridge tiles with ridge clips2
    BeforeAfter
    1. six tiles gone
    2. water in the attic

    Tuindorp

    Emergency cover after a storm, tiles replaced

    Area
    12 m²
    Duration
    1 day + 1 day
    Material
    Concrete tiles

    Before

    After a storm, six tiles were lying in the yard. Water in the attic.

    After

    Covered with a tarp the same afternoon. Two days later, new tiles laid and the ridge secured again.

    New build-up, top to bottom

    • Concrete tiles, 10 per m², on 22 × 32 mm battens
    • Counter battens on the existing roof board
    • Ridge tiles on a ridge roll, secured with ridge clips
  5. water pools here1drain sits above the puddle2damp patch in upstairs flat3
    PVC 1.5 mm, mechanically fixed1tapered insulation to the drain2two new drains3
    BeforeAfter
    1. water pools here
    2. drain sits above the puddle
    3. damp patch in upstairs flat

    Overvecht

    Flat roof of an apartment block replaced

    Area
    95 m²
    Duration
    4 days
    Material
    PVC

    Before

    The owners' association roof had puddles that stayed for days. Two top-floor apartments with damp patches.

    After

    Improved the slope with custom-cut insulation, new PVC covering and two extra drains.

    New build-up, top to bottom

    • PVC 1.5 mm, mechanically fastened, seams hot-air welded
    • PIR tapered boards 80 to 120 mm, at least 1.6% toward the drain
    • Two new drains Ø 100 mm with leaf guard
    • Vapor barrier on the concrete deck
  6. gutter corner leaks1green stains on the wall2
    zinc gutter 0.8 mm1downspout Ø 80 mm2
    BeforeAfter
    1. gutter corner leaks
    2. green stains on the wall

    Zuilen

    Gutter and dormer flashing renewed

    Area
    14 m²
    Duration
    1 day
    Material
    Zinc

    Before

    The zinc gutter leaked at the corners, and the wall below was turning green.

    After

    New zinc gutter, new corner pieces, and the joint between the dormer and the roof tiles checked.

    New build-up, top to bottom

    • Zinc box gutter 0.8 mm with bead
    • Corner pieces newly soldered
    • Gutter brackets every 50 cm
    • Zinc downspout Ø 80 mm

Your roof here?